ASTM A336 F11 Alloy Fittings – A336 Gr F11 Alloy Steel Forgings
ASC LLP, Mumbai, supplies ASTM A336 F11 alloy fittings and forgings: forged fittings, flanges, hubs, rings, discs and custom forgings in 1¼Cr-½Mo alloy steel, Class 1, 2 or 3. In addition, every forging comes with an EN 10204 3.1 certificate. See also our full range of alloy steel fittings.
What is ASTM A336 F11?
ASTM A336 (ASME SA336) is the specification for alloy steel forgings for pressure and high-temperature parts. Within it, Grade F11 is a 1¼% chromium – ½% molybdenum steel with added silicon. As a result, A336 F11 forgings keep their strength at temperature, so they are used for heavy boiler, pressure vessel and piping components.
A336 is mainly used for large or special forgings, such as vessel shells, heads, tubesheets, hubs, nozzles and big flanges. By contrast, standard small-bore forged fittings and B16.5 flanges are usually ordered to ASTM A182 F11, while buttweld elbows and tees are ordered to A234 WP11. For this reason, A336 F11 alloy fittings are typically heavy-wall, large-size or made to drawing.
ASTM A336 F11 – Quick Facts
- Specification: ASTM A336 / ASME SA336, Grade F11 Class 1, 2 or 3
- Composition: 1.00–1.50% Cr, 0.44–0.65% Mo and 0.50–1.00% Si
- Strength: 415–585 MPa (Class 1), up to 515–690 MPa (Class 3)
- Heat treatment: annealed, or normalised and then tempered at 620 °C min
- Products: forged fittings, flanges, rings, discs, shells and custom forgings

ASTM A336 F11 Chemical Composition
| Element (%) | F11 Class 1 | F11 Class 2 & 3 |
| Carbon (C) | 0.05 – 0.15 | 0.10 – 0.20 |
| Manganese (Mn) | 0.30 – 0.60 | 0.30 – 0.80 |
| Phosphorus (P) | 0.025 max | 0.025 max |
| Sulphur (S) | 0.025 max | 0.025 max |
| Silicon (Si) | 0.50 – 1.00 | 0.50 – 1.00 |
| Chromium (Cr) | 1.00 – 1.50 | 1.00 – 1.50 |
| Molybdenum (Mo) | 0.44 – 0.65 | 0.45 – 0.65 |
A336 sets tighter phosphorus and sulphur limits (0.025% max) than A182, because large forgings need cleaner steel. In addition, Classes 2 and 3 allow more carbon and manganese than Class 1, which gives them their higher strength.
ASTM A336 F11 Mechanical Properties – Class 1, 2 & 3
| Class | Tensile (MPa) | Yield, min (MPa) | Elong. / RA, min |
| Class 1 | 415 – 585 (60 – 85 ksi) | 205 (30 ksi) | 20% / 45% |
| Class 2 | 485 – 660 (70 – 95 ksi) | 275 (40 ksi) | 20% / 40% |
| Class 3 | 515 – 690 (75 – 100 ksi) | 310 (45 ksi) | 18% / 40% |
Unlike A182, A336 sets both a minimum and a maximum tensile strength for each class. Therefore, always state the class on the order, for example “ASTM A336 F11 Class 2”. A336 has no hardness or impact requirement for F11; however, buyers often add them for critical parts.


ASTM A336 F11 Heat Treatment
- Permitted treatments: forgings are annealed, or normalised and then tempered; liquid quenching and tempering is also allowed if agreed.
- Tempering temperature: at least 620 °C (1150 °F) for all F11 classes, so the forging reaches a stable, tough structure.
- Thick sections: in addition, heavy forgings are rough-machined before heat treatment where needed, so properties are uniform through the section.
A336 F11 vs A182 F11 vs A234 WP11
| Specification | Typical product | When to choose it |
| ASTM A336 F11 | Large and heavy forgings, as well as custom forged fittings | Heavy-wall, large size or made to drawing |
| ASTM A182 F11 | B16.11 forged fittings, B16.5 flanges | Standard small-bore fittings and flanges |
| ASTM A234 WP11 | Buttweld elbows, tees, reducers, caps | Standard buttweld fittings for P11 pipe |
All three share the same 1¼Cr-½Mo family. However, they cover different product forms, so the right specification depends on the size and shape of the part.
ASTM A336 F11 Alloy Fittings Specifications
| Item | Details |
| Specification | ASTM A336 / ASME SA336, Grade F11 Class 1, 2 or 3 |
| Products | Forged fittings, flanges, hubs, nozzles, rings, discs, shells, tubesheets and custom forgings |
| Size | As per drawing; in addition, rough or finish machined |
| Heat treatment | Annealed, or normalised and tempered (620 °C min temper) |
| Testing | Chemistry and tensile; also UT to ASTM A388, hardness and impact on request |
| Certificate | EN 10204 3.1; also 3.2 and third-party inspection on request |
A336 F11 Matching Grades
| Product form | Matching 1¼Cr-½Mo grade |
| Seamless pipe | ASTM A335 P11, so the piping matches |
| Forged fittings (standard) | ASTM A182 F11 |
| Flanges | ASTM A182 F11 flanges |
| Buttweld fittings | ASTM A234 WP11 |
| Plate | ASME SA387 Grade 11 |
| Valve castings | ASTM A217 WC6, as well as matching valve bodies |
Because these grades share the same chemistry family, a P11 system can combine A336 forgings with standard fittings, flanges and plate. Welding F11, however, needs care: it is a P-No. 4 material, so it requires preheat, B2 filler metal and post-weld heat treatment.
Applications of ASTM A336 F11 Alloy Fittings
| Industry | Typical A336 F11 use |
| Power generation | Boiler headers, drum forgings and turbine casing parts, as well as heavy nozzles |
| Refining & petrochemical | Reactor and vessel forgings, while temperatures stay below about 565 °C |
| Pressure vessels | Shells, heads and tubesheets in Cr-Mo service |
| Heat exchangers | Tubesheets and channel forgings, for example on Cr-Mo exchangers |
A336 F11 forgings are often used with heat exchangers and boiler equipment. However, F11 is a low-alloy steel, not a stainless steel, so wet corrosive service needs stainless or clad parts instead.
A336 F11 vs Other ASTM A336 Grades
| A336 grade | Composition | Typical use |
| F1 | C – ½Mo | Moderate-temperature forgings, since it has no chromium |
| F11 | 1¼Cr – ½Mo – Si | Steam service, while temperatures stay below about 565 °C |
| F12 | 1Cr – ½Mo | Similar to F11; however, silicon is lower |
| F22 | 2¼Cr – 1Mo | Hydrogen service up to about 595 °C |
| F5 | 5Cr – ½Mo | Sulphur and hydrogen service |
| F91 | 9Cr – 1Mo – V | Highest creep strength |
In short, chromium content rises from F1 to F91, and so does high-temperature capability. See also our alloy steel products.
Why Buy ASTM A336 F11 Forgings from ASC LLP?
- Traceable material: EN 10204 3.1 certificates with chemistry, heat treatment and tensile results.
- Made to drawing: forgings supplied rough or finish machined, so they are ready for fabrication.
- Testing: UT to A388, hardness and impact tests; in addition, third-party inspection on request.
- Correct grade advice: help choosing A336, A182 or A234, because size and shape decide the specification.
Frequently Asked Questions – ASTM A336 F11 Alloy Fittings
What is ASTM A336 F11?
In short, ASTM A336 F11 is a 1¼Cr-½Mo alloy steel for forgings used in pressure and high-temperature parts, such as forged fittings, flanges, shells and tubesheets.
What is the chemical composition of A336 F11?
Class 1 has C 0.05–0.15% and Mn 0.30–0.60%, while Classes 2 and 3 have C 0.10–0.20% and Mn 0.30–0.80%. In addition, all classes have Cr 1.00–1.50%, Si 0.50–1.00% and P / S 0.025% max.
What are the mechanical properties of A336 F11?
Class 1 is 415–585 MPa tensile and 205 MPa yield, Class 2 is 485–660 / 275 MPa, and Class 3 is 515–690 / 310 MPa.
What is the difference between A336 F11 and A182 F11?
Both are 1¼Cr-½Mo forgings. However, A336 is mainly used for large and heavy forgings with tighter P and S limits, whereas A182 covers standard forged fittings and flanges.
What heat treatment does A336 F11 need?
A336 F11 is annealed, or normalised and tempered, at a minimum tempering temperature of 620 °C (1150 °F).
Which pipe is used with A336 F11 forgings?
They are normally used with ASTM A335 P11 seamless pipe, together with A182 F11 fittings and A234 WP11 buttweld fittings.
Is A336 F11 corrosion resistant?
No. F11 resists oxidation at high temperature, but it is not stainless steel, so it is not used for wet corrosive service.
Global Supply
ASC LLP supplies ASTM A336 F11 alloy fittings and forgings from Mumbai to customers in India, the Middle East, Europe, Africa, the Americas and South-East Asia. To get a prompt quotation, simply send your drawing or enquiry with class, size, testing and quantity.

Countries We Export To
UNITED STATES, EUROPE, UK, UAE, SAUDI ARABIA, OMAN, KUWAIT, JORDAN, QATAR, INDONESIA, MALAYSIA, BRAZIL, SPAIN, ITALY, FRANCE, GERMANY, BAHRAIN, SRI LANKA, AZERBAIJAN, AUSTRALIA, AUSTRIA, PHILIPPINES, TURKEY, RUSSIA, IRAN, IRAQ, CANADA, KOREA, JAPAN, YEMEN, FINLAND, ZIMBABWE, HUNGARY, PORTUGAL, VIETNAM, MOROCCO, THAILAND, SOUTH AFRICA, MEXICO, SINGAPORE, GREECE, KUWAIT, POLAND, NEW ZEALAND, SWEDEN, SWITZERLAND, BELGIUM, BHUTAN, BANGLADESH, TAIWAN, ROMANIA, CAMBODIA, KAZAKHSTAN, AFGHANISTAN.