ASTM A335 P11 Alloy Steel Pipes – ASME SA335 P11 (1¼Cr-½Mo, UNS K11597)

ASC LLP, Mumbai, supplies ASTM A335 P11 pipe (ASME SA335 P11, UNS K11597) – seamless 1¼% chromium, ½% molybdenum alloy steel pipe for high-temperature steam and refinery service. It comes in ½” to 24″ NB, SCH 40 to XXS, with EN 10204 3.1 certificates. See our alloy steel seamless pipe range.

What is P11 Material?

P11 is a chrome-moly (Cr-Mo) low-alloy steel to ASTM A335, the specification for seamless ferritic alloy steel pipe for high-temperature service. It contains about 1¼% chromium, ½% molybdenum and 0.5 – 1.0% silicon. Molybdenum gives creep strength at high temperature. Chromium and silicon improve resistance to oxidation and scaling, and chromium also helps resist hydrogen attack in refinery service. Compared with carbon steel such as A106 B, P11 keeps its strength at higher temperatures and does not suffer graphitisation. It is used for steam lines and refinery piping up to about 550 °C.

The same 1¼Cr-½Mo material is called T11 as tube (ASTM A213 T11), F11 as forgings and flanges, WP11 as butt-weld fittings and Grade 11 as plate.

ASTM A335 P11 seamless alloy steel pipe

P11 Material Chemical Composition (UNS K11597)

Element ASTM A335 P11 (%)
Carbon (C) 0.05 – 0.15
Manganese (Mn) 0.30 – 0.60
Phosphorus (P) 0.025 max.
Sulphur (S) 0.025 max.
Silicon (Si) 0.50 – 1.00
Chromium (Cr) 1.00 – 1.50
Molybdenum (Mo) 0.44 – 0.65

The relatively high silicon (0.50 – 1.00%) distinguishes P11 from P12 (1Cr-½Mo, lower silicon) and adds to its oxidation resistance.

Heat Treatment, Welding & PWHT

  • Mill heat treatment (A335): full or isothermal anneal, or normalise and temper with tempering at 650 °C (1200 °F) minimum.
  • Welding: P11 is a P-No. 4 material. Typical practice is a preheat of about 150 °C and matching 1¼Cr-½Mo filler metal.
  • PWHT: post-weld heat treatment, typically around 700 – 750 °C, is required above code thickness limits – follow ASME B31.1 / B31.3 and the project specification.

Read more: heat treatment of P11 pipe.

ASTM A335 P5, P9, P11, P22, P91 alloy steel seamless pipes
A335 Gr P11 alloy steel seamless pipes

ASTM A335 P11 Pipe Schedule & Weight Chart (ASME B36.10M)

NPS OD (mm) SCH 40 (mm) SCH 80 (mm) SCH 160 (mm) XXS (mm) SCH 40 kg/m SCH 80 kg/m
½” 21.34 2.77 3.73 4.78 7.47 1.27 1.62
¾” 26.67 2.87 3.91 5.56 7.82 1.68 2.19
1″ 33.40 3.38 4.55 6.35 9.09 2.50 3.24
1¼” 42.16 3.56 4.85 6.35 9.70 3.39 4.46
1½” 48.26 3.68 5.08 7.14 10.15 4.05 5.41
2″ 60.33 3.91 5.54 8.74 11.07 5.44 7.49
2½” 73.03 5.16 7.01 9.53 14.02 8.64 11.41
3″ 88.90 5.49 7.62 11.13 15.24 11.29 15.27
4″ 114.30 6.02 8.56 13.49 17.12 16.07 22.32
5″ 141.30 6.55 9.53 15.88 19.05 21.77 30.97
6″ 168.28 7.11 10.97 18.26 21.95 28.26 42.56
8″ 219.08 8.18 12.70 23.01 22.23 42.54 64.63
10″ 273.05 9.27 15.09 28.58 25.40 60.30 95.99
12″ 323.85 10.31 17.48 33.32 25.40 79.72 132.06
14″ 355.60 11.13 19.05 35.71 – 94.55 158.10
16″ 406.40 12.70 21.44 40.49 – 123.30 203.53
18″ 457.20 14.27 23.83 45.24 – 155.87 254.67
20″ 508.00 15.09 26.19 50.01 – 183.42 311.17
24″ 609.60 17.48 30.96 59.54 – 255.24 441.78

Plain-end weights calculated at 7.85 g/cm³. Other schedules (SCH 10 – 140) and specified walls on request; ⅛” – ⅜” and over 24″ available to order.

Mechanical Properties of A335 P11 Pipe

Property ASTM A335 P11
Tensile strength, min. 415 MPa (60 ksi)
Yield strength, min. 205 MPa (30 ksi)
Elongation, longitudinal / transverse (basic min.) 30% / 20%
Elongation, round 50 mm or 4D specimen 22% / 14%
Hardness Not specified by A335 for P11 (limits may be set by the purchaser)

Basic elongation applies to wall 8 mm (5/16″) and over; lower values apply to thinner strip specimens.

P11 vs P12, P22, P5 & P91

Grade Nominal composition Tensile / yield min. (MPa) Typical use
P12 1Cr-½Mo 415 / 220 Steam lines, similar to P11
P11 1¼Cr-½Mo-Si 415 / 205 Steam lines, headers and refinery piping to about 550 °C
P22 2¼Cr-1Mo 415 / 205 Higher creep strength, hydrogen service
P5 5Cr-½Mo 415 / 205 Refinery service with sulphur corrosion
P91 9Cr-1Mo-V-Nb 585 / 415 Main steam and hot reheat at 550 – 600 °C

Comparison guide: P5 vs P11 vs P91 – which to choose.

A335 P11 Pipe Specifications

Item Details
Specification ASTM A335 / ASME SA335, Grade P11
UNS K11597
Type Seamless – hot finished or cold drawn
Size ½” – 24″ NB (⅛” – ⅜” and larger sizes on request)
Wall SCH 10 – XXS, STD, XS or specified wall
Length Single random, double random, cut lengths
Ends Plain or bevelled for butt welding
Heat treatment Annealed, or normalised and tempered (650 °C min.)
Testing Tension, flattening / bend, hydro or NDE, PMI; hardness and UT on request
Certificate EN 10204 3.1 / 3.2

Physical Properties of P11

Property Value (approx., at 20 °C)
Density 7.85 g/cm³
Modulus of elasticity ≈ 205 GPa
Thermal conductivity ≈ 42 W/m·K
Magnetic Yes (ferritic)

P11 Equivalent Grades

Standard Equivalent / related grade
ASTM / ASME A335 / SA335 P11 (K11597)
EN 10216-2 13CrMo4-5 (1.7335) – nearest
JIS G3458 STPA23
Tube ASTM A213 T11
Forgings / flanges / fittings ASTM A182 F11, A336 F11, A234 WP11
Plate ASTM A387 Grade 11

Equivalents are similar but not identical in chemistry and testing – confirm with the design code before substituting.

Applications of ASTM A335 P11 Pipes

Industry Typical P11 pipe applications
Power plants Steam lines, headers, reheat and auxiliary steam piping
Refineries Furnace and heater piping, hydrotreater and reformer lines
Petrochemical plants High-temperature process piping
Industrial boilers Superheated steam distribution

For boiler and heat-exchanger tubes use T11 tubes. More: P11 pipes in power plants.

Why Buy P11 Pipe from ASC LLP?

Send size, schedule, length and quantity to sales@amardeepsteel.com, call 022-67439130 or contact us.

Frequently Asked Questions – ASTM A335 P11 Pipe

What is P11 material?

P11 is a 1¼% chromium, ½% molybdenum low-alloy steel (UNS K11597) used for seamless pipe to ASTM A335 / ASME SA335. It is used for high-temperature steam and refinery piping where carbon steel would lose strength.

What is the chemical composition of P11?

ASTM A335 P11 contains C 0.05–0.15%, Mn 0.30–0.60%, P 0.025% max., S 0.025% max., Si 0.50–1.00%, Cr 1.00–1.50% and Mo 0.44–0.65%.

What are the mechanical properties of A335 P11 pipe?

Minimum tensile strength is 415 MPa (60 ksi) and minimum yield strength is 205 MPa (30 ksi). Basic minimum elongation is 30% longitudinal and 20% transverse.

What is the heat treatment for P11 pipe?

A335 P11 pipe is supplied full or isothermal annealed, or normalised and tempered with a minimum tempering temperature of 650 °C (1200 °F).

What is the difference between P11 and P22?

P11 contains about 1¼% Cr and ½% Mo, while P22 contains about 2¼% Cr and 1% Mo. P22 has higher creep strength at high temperature; both have the same minimum tensile and yield strength at room temperature.

What is the equivalent of A335 P11?

The nearest European equivalent is EN 10216-2 13CrMo4-5 (1.7335) and the Japanese equivalent is JIS STPA23. The matching tube grade is A213 T11, fittings A234 WP11 and forgings/flanges A182 F11.

For sizes 16″ and above, P11 chemistry is also supplied as electric-fusion-welded pipe: see our ASTM A691 1-1/4CR Class 22 EFW pipe page.

Global Reach

ASC LLP supplies alloy steel pipes, fittings and flanges to power, refinery and EPC customers in the USA, Europe, the Middle East and Asia, with secure packing and full documentation. Buyers worldwide rely on our ASTM A335 P11 alloy steel pipes for certified material and traceability.

ASC LLP global export of ASTM A335 P11 pipes

Countries We Export To

UNITED STATES, EUROPE, UK, UAE, SAUDI ARABIA, OMAN, KUWAIT, JORDAN, QATAR, INDONESIA, MALAYSIA, BRAZIL, SPAIN, ITALY, FRANCE, GERMANY, BAHRAIN, SRI LANKA, AZERBAIJAN, AUSTRALIA, AUSTRIA, PHILIPPINES, TURKEY, RUSSIA, IRAN, IRAQ, CANADA, KOREA, JAPAN, YEMEN, FINLAND, ZIMBABWE, HUNGARY, PORTUGAL, VIETNAM, MOROCCO, THAILAND, SOUTH AFRICA, MEXICO, SINGAPORE, GREECE, KUWAIT, POLAND, NEW ZEALAND, SWEDEN, SWITZERLAND, BELGIUM, BHUTAN, BANGLADESH, TAIWAN, ROMANIA, CAMBODIA, KAZAKHSTAN, AFGHANISTAN.

Follow us on: