ASTM A335 P22 Alloy Seamless Pipes – ASME SA335 P22 (2¼Cr-1Mo, UNS K21590)

ASC LLP, Mumbai, supplies ASTM A335 P22 pipe (ASME SA335 P22, UNS K21590): seamless 2¼% chromium, 1% molybdenum alloy steel pipe for high-temperature steam and hydrogen service. Sizes run from ½” to 24″ NB, SCH 40 to XXS, with EN 10204 3.1 certificates. See our alloy steel seamless pipe range.

What is P22 Material?

P22 is a 2¼Cr-1Mo chrome-moly low-alloy steel made to ASTM A335, the specification for seamless ferritic alloy steel pipe for high-temperature service. Compared with P11 (1¼Cr-½Mo), its higher molybdenum gives P22 greater creep strength at 500 – 600 °C. Its chromium gives better resistance to oxidation and to high-temperature hydrogen attack, which is why 2¼Cr-1Mo is a standard material for refinery hydroprocessing units. It is also widely used for steam lines and headers in power plants.

The same 2¼Cr-1Mo material is called T22 as tube (ASTM A213 T22), F22 as forgings and flanges, WP22 as butt-weld fittings and Grade 22 as plate.

ASTM A335 P22 alloy steel seamless pipe

P22 Material Chemical Composition (UNS K21590)

Element ASTM A335 P22 (%)
Carbon (C) 0.05 – 0.15
Manganese (Mn) 0.30 – 0.60
Phosphorus (P) 0.025 max.
Sulphur (S) 0.025 max.
Silicon (Si) 0.50 max.
Chromium (Cr) 1.90 – 2.60
Molybdenum (Mo) 0.87 – 1.13

Nominal composition: 2¼% Cr, 1% Mo. Compare P11 (1.00 – 1.50% Cr, 0.44 – 0.65% Mo, 0.50 – 1.00% Si).

Heat Treatment, Welding & PWHT

  • Mill heat treatment (A335): full or isothermal anneal, or normalise and temper, with tempering at 675 °C (1250 °F) minimum.
  • Welding: P22 is a P-No. 5A material. Typical practice is a preheat of about 150 – 200 °C and matching 2¼Cr-1Mo filler metal.
  • PWHT: post-weld heat treatment, typically around 700 – 760 °C, is normally required. Follow ASME B31.1 / B31.3 and the project specification, including hardness checks for hydrogen or sour service.
ASTM A335 P22 pipe
Alloy steel ASTM A335 P22 pipes

ASTM A335 P22 Pipe Schedule & Weight Chart (ASME B36.10M)

NPS OD (mm) SCH 40 (mm) SCH 80 (mm) SCH 160 (mm) XXS (mm) SCH 40 kg/m SCH 80 kg/m
½” 21.34 2.77 3.73 4.78 7.47 1.27 1.62
¾” 26.67 2.87 3.91 5.56 7.82 1.68 2.19
1″ 33.40 3.38 4.55 6.35 9.09 2.50 3.24
1¼” 42.16 3.56 4.85 6.35 9.70 3.39 4.46
1½” 48.26 3.68 5.08 7.14 10.15 4.05 5.41
2″ 60.33 3.91 5.54 8.74 11.07 5.44 7.49
2½” 73.03 5.16 7.01 9.53 14.02 8.64 11.41
3″ 88.90 5.49 7.62 11.13 15.24 11.29 15.27
4″ 114.30 6.02 8.56 13.49 17.12 16.07 22.32
5″ 141.30 6.55 9.53 15.88 19.05 21.77 30.97
6″ 168.28 7.11 10.97 18.26 21.95 28.26 42.56
8″ 219.08 8.18 12.70 23.01 22.23 42.54 64.63
10″ 273.05 9.27 15.09 28.58 25.40 60.30 95.99
12″ 323.85 10.31 17.48 33.32 25.40 79.72 132.06
14″ 355.60 11.13 19.05 35.71 – 94.55 158.10
16″ 406.40 12.70 21.44 40.49 – 123.30 203.53
18″ 457.20 14.27 23.83 45.24 – 155.87 254.67
20″ 508.00 15.09 26.19 50.01 – 183.42 311.17
24″ 609.60 17.48 30.96 59.54 – 255.24 441.78

Plain-end weights calculated at 7.85 g/cm³. XXS is not standard above 12″. Other schedules (SCH 10 – 140), specified walls and sizes over 24″ on request.

Mechanical Properties of A335 P22 Pipe

Property ASTM A335 P22
Tensile strength, min. 415 MPa (60 ksi)
Yield strength, min. 205 MPa (30 ksi)
Elongation, longitudinal / transverse (basic min.) 30% / 20%
Elongation, round 50 mm or 4D specimen 22% / 14%
Hardness Not specified by A335 for P22 (limits may be set by the purchaser, e.g. for hydrogen or sour service)

A335 P22 Pipe Specifications

Item Details
Specification ASTM A335 / ASME SA335, Grade P22
UNS K21590
Type Seamless, hot finished or cold drawn
Size ½” – 24″ NB (smaller and larger sizes on request)
Wall SCH 10 – XXS, STD, XS or specified wall
Length Single random, double random, cut lengths
Ends Plain or bevelled for butt welding
Heat treatment Annealed, or normalised and tempered (675 °C min.)
Testing Tension, flattening / bend, hydro or NDE, PMI; hardness, UT and impact on request
Certificate EN 10204 3.1 / 3.2

P22 vs P11, P5, P9 & P91

Grade Nominal composition Tensile / yield min. (MPa) Typical use
P11 1¼Cr-½Mo-Si 415 / 205 Steam lines and refinery piping to about 550 °C
P22 2¼Cr-1Mo 415 / 205 Higher creep strength; hydrogen service
P5 5Cr-½Mo 415 / 205 Refinery service with sulphur corrosion
P9 9Cr-1Mo 415 / 205 Heater tubes and piping in high-sulphur service
P91 9Cr-1Mo-V-Nb 585 / 415 Main steam and hot reheat at 550 – 600 °C

For ultra-supercritical steam lines see P92.

P22 Equivalent Grades

Standard Equivalent / related grade
ASTM / ASME A335 / SA335 P22 (K21590)
EN 10216-2 10CrMo9-10 (1.7380)
JIS G3458 STPA24
Tube ASTM A213 T22
Forgings / flanges / fittings ASTM A182 F22, A336 F22, A234 WP22
Plate ASTM A387 Grade 22

Equivalents are similar, not identical; confirm with the design code before substituting.

Applications of ASTM A335 P22 Pipes

Industry Typical P22 pipe applications
Power plants Main and auxiliary steam lines, headers, hot reheat piping
Refineries Hydrotreater, hydrocracker and reformer piping (hydrogen service)
Petrochemical plants High-temperature process and heater piping
Industrial boilers Superheated steam distribution

For boiler and heat-exchanger tubes use T22 tubes.

Physical Properties of P22

Property Value (approx., at 20 °C)
Density 7.85 g/cm³
Modulus of elasticity ≈ 210 GPa
Thermal conductivity ≈ 36 W/m·K
Magnetic Yes (ferritic)

Why Buy P22 Pipe from ASC LLP?

  • Correct paperwork: A335 / SA335 P22 with EN 10204 3.1 certificates showing heat treatment, chemistry and tensile results.
  • PMI checked: positive material identification before dispatch, to avoid mix-ups with P11 or carbon steel.
  • Complete P22 system: pipe, fittings, flanges, forgings, tubes and plate from one source.
  • Export packing with bevel protectors and end caps.

Send size, schedule, length and quantity to sales@amardeepsteel.com, call 022-67439130 or contact us.

Frequently Asked Questions – ASTM A335 P22 Pipe

What is P22 material?

P22 is a 2¼% chromium, 1% molybdenum low-alloy steel (UNS K21590) used for seamless pipe to ASTM A335 / ASME SA335. It is used for high-temperature steam piping and refinery hydrogen service.

What is the chemical composition of P22?

ASTM A335 P22 contains C 0.05–0.15%, Mn 0.30–0.60%, P 0.025% max., S 0.025% max., Si 0.50% max., Cr 1.90–2.60% and Mo 0.87–1.13%.

What are the mechanical properties of A335 P22 pipe?

Minimum tensile strength is 415 MPa (60 ksi) and minimum yield strength 205 MPa (30 ksi). Basic minimum elongation is 30% longitudinal and 20% transverse.

What is the heat treatment for P22 pipe?

A335 P22 pipe is supplied full or isothermal annealed, or normalised and tempered with a minimum tempering temperature of 675 °C (1250 °F).

What is the difference between P11 and P22?

P22 contains about 2¼% Cr and 1% Mo, while P11 contains about 1¼% Cr and ½% Mo plus 0.5–1.0% Si. P22 has higher creep strength and better resistance to hydrogen attack; both have the same minimum room-temperature tensile and yield strength.

What is the equivalent of A335 P22?

The European equivalent is EN 10216-2 10CrMo9-10 (1.7380) and the Japanese equivalent is JIS STPA24. Matching grades are A213 T22 tube, A234 WP22 fittings, A182 F22 forgings and A387 Grade 22 plate.

Global Reach

ASC LLP supplies alloy steel pipes, fittings and flanges to power, refinery and EPC customers in the USA, Europe, the Middle East and Asia, with secure packing and full documentation. Buyers worldwide rely on our ASTM A335 P22 alloy seamless pipes for certified material and traceability.

ASC LLP global export of ASTM A335 P22 pipes

Countries We Export To

UNITED STATES, EUROPE, UK, UAE, SAUDI ARABIA, OMAN, KUWAIT, JORDAN, QATAR, INDONESIA, MALAYSIA, BRAZIL, SPAIN, ITALY, FRANCE, GERMANY, BAHRAIN, SRI LANKA, AZERBAIJAN, AUSTRALIA, AUSTRIA, PHILIPPINES, TURKEY, RUSSIA, IRAN, IRAQ, CANADA, KOREA, JAPAN, YEMEN, FINLAND, ZIMBABWE, HUNGARY, PORTUGAL, VIETNAM, MOROCCO, THAILAND, SOUTH AFRICA, MEXICO, SINGAPORE, GREECE, KUWAIT, POLAND, NEW ZEALAND, SWEDEN, SWITZERLAND, BELGIUM, BHUTAN, BANGLADESH, TAIWAN, ROMANIA, CAMBODIA, KAZAKHSTAN, AFGHANISTAN.