ASTM A335 P92 Alloy Seamless Pipes – ASME SA335 P92 (9Cr-0.5Mo-1.8W, UNS K92460)

ASC LLP, Mumbai, supplies ASTM A335 P92 pipe (ASME SA335 P92, UNS K92460). This is seamless 9Cr-0.5Mo-1.8W-V-Nb alloy steel pipe for main steam and hot reheat lines in supercritical and ultra-supercritical power plants. We supply ½” to 24″ NB, normalised and tempered, with EN 10204 3.1 certificates. See our alloy steel seamless pipe range.

What is ASTM A335 P92?

P92 is a creep-strength-enhanced ferritic (CSEF) steel developed from P91. Part of the molybdenum is replaced by about 1.8% tungsten, and small amounts of boron, niobium, vanadium and nitrogen are added. The result is about 10 – 20% higher creep strength than P91 at 600 – 620 °C. This lets designers use thinner pipe walls for high-pressure, high-temperature steam lines, which reduces weight, support loads and thermal stress.

406 mm ASTM A335 P92 seamless pipes

P92 Chemical Composition (UNS K92460)

Element ASTM A335 P92 (%)
Carbon (C) 0.07 – 0.13
Manganese (Mn) 0.30 – 0.60
Phosphorus (P) 0.020 max.
Sulphur (S) 0.010 max.
Silicon (Si) 0.50 max.
Chromium (Cr) 8.50 – 9.50
Molybdenum (Mo) 0.30 – 0.60
Tungsten (W) 1.50 – 2.00
Vanadium (V) 0.15 – 0.25
Niobium (Nb) 0.04 – 0.09
Nitrogen (N) 0.030 – 0.070
Boron (B) 0.001 – 0.006
Nickel (Ni) 0.40 max.
Aluminium (Al) 0.02 max.
Titanium (Ti) 0.01 max.
Zirconium (Zr) 0.01 max.

Heat-analysis limits per ASTM A335 / ASME SA335 Grade P92. Compared with P91, P92 has less Mo (0.30 – 0.60% vs 0.85 – 1.05%), adds W and B, and has a narrower Nb range.

Why Tungsten and Boron?

  • Tungsten (1.5 – 2.0%) strengthens the iron matrix and slows the coarsening of carbides at service temperature – the main reason for P92’s higher creep strength.
  • Boron (10 – 60 ppm) stabilises the fine carbides along grain boundaries, improving long-term creep life.
  • Vanadium, niobium and nitrogen form fine carbonitrides, as in P91.
  • 9% chromium gives steam-side oxidation resistance similar to P91.
Alloy steel ASTM A335 P92 pipe
ASTM A335 P92 alloy seamless pipe

ASTM A335 P92 Pipe – Technical Data

P92 Pipe Size, Schedule & Weight Chart (ASME B36.10M, wall in mm)

NPS OD (mm) SCH 40 SCH 80 SCH 160 XXS SCH 80 kg/m SCH 160 kg/m
½” 21.34 2.77 3.73 4.78 7.47 1.60 1.93
¾” 26.67 2.87 3.91 5.56 7.82 2.17 2.86
1″ 33.40 3.38 4.55 6.35 9.09 3.20 4.19
1½” 48.26 3.68 5.08 7.14 10.15 5.35 7.17
2″ 60.33 3.91 5.54 8.74 11.07 7.41 11.01
3″ 88.90 5.49 7.62 11.13 15.24 15.12 21.13
4″ 114.30 6.02 8.56 13.49 17.12 22.09 33.19
6″ 168.28 7.11 10.97 18.26 21.95 42.12 66.86
8″ 219.08 8.18 12.70 23.01 22.23 63.98 110.12
10″ 273.05 9.27 15.09 28.58 25.40 95.01 170.54
12″ 323.85 10.31 17.48 33.32 25.40 130.72 236.29
14″ 355.60 11.13 19.05 35.71 – 156.49 278.83
16″ 406.40 12.70 21.44 40.49 – 201.46 361.63
18″ 457.20 14.27 23.83 45.24 – 252.07 454.91
20″ 508.00 15.09 26.19 50.01 – 308.00 559.06
24″ 609.60 17.48 30.96 59.54 – 437.27 799.40

Plain-end weights calculated for P92 density (≈ 7.77 g/cm³). P92 main steam lines are often ordered to calculated minimum wall (MW) or ID-controlled (ID × MW) dimensions rather than schedules – state the basis on your enquiry.

Mechanical Properties of A335 P92 Pipe

Property ASTM A335 P92
Tensile strength, min. 620 MPa (90 ksi)
Yield strength, min. 440 MPa (64 ksi)
Elongation in 50 mm, min. 20% longitudinal / 13% transverse
Hardness 250 HBW max. (check the current A335 edition for the minimum)

Elevated-temperature allowable stresses are given in ASME Section II-D and the piping codes – use those, not room-temperature values, for design.

A335 P92 Pipe Specifications

Item Details
Specification ASTM A335 / ASME SA335, Grade P92
UNS K92460
Type Seamless, hot finished
Size ½” – 24″ NB; larger and ID-controlled sizes on request
Wall SCH 40 – XXS, or calculated minimum wall
Heat treatment Normalised 1040 – 1080 °C + tempered 730 – 800 °C
Testing Tension, flattening / bend, hardness, hydro or NDE, UT, PMI
Certificate EN 10204 3.1 / 3.2

P92 vs P91 vs P22

Grade Nominal composition Tensile / yield min. (MPa) Typical use
P22 2¼Cr-1Mo 415 / 205 Steam lines to about 550 °C
P91 9Cr-1Mo-V-Nb 585 / 415 Main steam / hot reheat to about 600 °C
P92 9Cr-0.5Mo-1.8W-V-Nb-B 620 / 440 Main steam / hot reheat in USC units, 600 – 620 °C

Heat Treatment, Welding & PWHT

  • Mill heat treatment: normalise at 1040 – 1080 °C, then temper at 730 – 800 °C.
  • Welding: qualified procedure with matching 9Cr-W filler, preheat about 200 – 250 °C, controlled interpass temperature, and cooling to complete transformation before PWHT.
  • PWHT: mandatory, typically around 745 – 775 °C, with hardness checks afterwards. Incorrect tempering or PWHT reduces creep life.

Physical Properties

Property Value (approx., at 20 °C)
Density ≈ 7.77 g/cm³
Modulus of elasticity ≈ 215 GPa
Thermal conductivity ≈ 26 W/m·K
Magnetic Yes (ferritic / martensitic)

P92 Equivalent Grades

Standard Equivalent / related grade
ASTM / ASME A335 / SA335 P92 (K92460)
EN 10216-2 X10CrWMoVNb9-2 (1.4901)
Tube ASTM A213 T92
Fittings / forgings A234 WP92, A182 F92

Applications of ASTM A335 P92 Pipes

Industry Typical P92 pipe applications
Supercritical & USC power plants Main steam, hot reheat and turbine bypass piping
Boiler headers Superheater and reheater outlet headers
HRSGs High-pressure steam headers and links

For superheater and reheater tubes use T92 tubes. P92 is not intended for marine, oil & gas production or corrosive chemical service.

Why Buy P92 Pipe from ASC LLP?

  • Correct paperwork: A335 / SA335 P92 with 3.1 certificates showing heat treatment, hardness and full chemistry including W, Nb, N and B.
  • Checks before dispatch: PMI to tell P92 from P91, hardness verification, UT and third-party inspection on request.
  • Calculated-wall and ID-controlled sizes for main steam lines.
  • Export packing with bevel protectors and end caps.

Send size, wall basis, length and quantity to sales@amardeepsteel.com, call 022-67439130 or contact us.

Frequently Asked Questions – ASTM A335 P92 Pipe

What is the chemical composition of P92?

ASTM A335 P92 contains C 0.07–0.13%, Mn 0.30–0.60%, Si 0.50% max., Cr 8.50–9.50%, Mo 0.30–0.60%, W 1.50–2.00%, V 0.15–0.25%, Nb 0.04–0.09%, N 0.030–0.070% and B 0.001–0.006%, with P 0.020% max., S 0.010% max. and Ni 0.40% max.

What is P92 material?

P92 (UNS K92460) is a 9Cr-0.5Mo-1.8W-V-Nb-B creep-strength-enhanced ferritic steel supplied as seamless pipe to ASTM A335 / ASME SA335. It is used for main steam and hot reheat piping in supercritical and ultra-supercritical power plants.

What are the mechanical properties of P92 pipe?

ASTM A335 P92 has a minimum tensile strength of 620 MPa (90 ksi), minimum yield strength of 440 MPa (64 ksi), and minimum elongation of 20% longitudinal or 13% transverse.

What is the difference between P91 and P92?

P92 replaces part of the molybdenum in P91 with about 1.8% tungsten and adds boron. This gives P92 higher strength (620/440 MPa vs 585/415 MPa) and about 10–20% higher creep strength at 600–620 °C, allowing thinner walls.

What is the heat treatment for P92 pipe?

P92 pipe is normalised at 1040–1080 °C and tempered at 730–800 °C. Post-weld heat treatment is mandatory after welding.

What is the equivalent of A335 P92?

The European equivalent is EN 10216-2 X10CrWMoVNb9-2 (1.4901). The matching tube grade is ASTM A213 T92, with A234 WP92 fittings and A182 F92 forgings.

Global Reach

ASC LLP supplies alloy steel pipes, tubes and fittings to power plants, boiler makers and EPC contractors in the USA, Europe, the Middle East and Asia, with secure packing and full documentation. Buyers worldwide rely on our ASTM A335 P92 alloy seamless pipes for certified material and traceability.

ASC LLP global export of ASTM A335 P92 pipes

Countries We Export To

UNITED STATES, EUROPE, UK, UAE, SAUDI ARABIA, OMAN, KUWAIT, JORDAN, QATAR, INDONESIA, MALAYSIA, BRAZIL, SPAIN, ITALY, FRANCE, GERMANY, BAHRAIN, SRI LANKA, AZERBAIJAN, AUSTRALIA, AUSTRIA, PHILIPPINES, TURKEY, RUSSIA, IRAN, IRAQ, CANADA, KOREA, JAPAN, YEMEN, FINLAND, ZIMBABWE, HUNGARY, PORTUGAL, VIETNAM, MOROCCO, THAILAND, SOUTH AFRICA, MEXICO, SINGAPORE, GREECE, KUWAIT, POLAND, NEW ZEALAND, SWEDEN, SWITZERLAND, BELGIUM, BHUTAN, BANGLADESH, TAIWAN, ROMANIA, CAMBODIA, KAZAKHSTAN, AFGHANISTAN.

Follow us on: